Cause
A paint defect as a result of an oil based paint coming in contact with an alkali surface which had a high moisture content at the time of painting and not completely sealed with an alkali resistant primer.
Remove the soft/sticky film, wash down with white spirit, and allow to dry then apply an alkali resistant primer followed by overcoating with an oil based system.